Customization: | Available |
---|---|
Casting Method: | Sand Casting or Special Casting |
Casting Form Material: | Metal |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
It is used in the roughing stands of round and sections, especially the BD2 mills for rail & beams.
Compared with other nodular iron rolls, NCC rolls have unique material and heat treatment process ensuring they are good enough to replace the traditional cast steel rolls but with a better life.
We control the carbide at a very low level (less than 5%) by reducing the chrome down to 0.3%, raising the silicon and applying isothermal quenching to make the carbide solid solution into the matrix.
Meanwhile, we can achieve a matrix of tempered sorbite/bainite by applying heat treatment d increasing nickel. This type of matrix has much better performance than the pearlite on the resistance of wear, fire crack and impact, especially the excellent red hardness thanks to the molybdenum.
Chemical Composition
Grade |
C |
Si |
Mn |
P |
S |
Cr |
Ni |
Mo |
NCC I |
3.00-3.40 |
2.00-2.50 |
0.80-1.00 |
≤0.10 |
≤0.030 |
≤0.15 |
2.00-3.00 |
0.40-0.70 |
NCC II |
3.00-3.40 |
1.50-2.00 |
0.80-1.00 |
≤0.10 |
≤0.030 |
≤0.15 |
2.50-4.50 |
0.50-1.00 |
Mechanical Properties
Tensile Strength (kg/mm²) |
≥520 |
Bending Strength (kg/mm²) |
970-1380 |
Elongation (%) |
0.2-0.5 |